EN 10025-6 S890QL, also written S890 QL, EN10025-6 S890QL and steel number 1.8983, is a weldable quenched and tempered structural steel, but weldability is a qualified-procedure issue, not an automatic property of the grade name. The notes below reuse the official welding and CEV wording already disclosed on EN 10025-6 S890QL, together with the official chemistry and strength tables.
EN 10025-6 S890QL Weldability — What Is Specified and What Is Practice
| Topic | Position used on this page |
|---|---|
| Official weldability statement | Can be welded, but needs more care than lower-strength structural steels. A qualified WPS following EN 1011-2, low-hydrogen consumables and controlled heat input are required, as stated on EN 10025-6 S890QL |
| Cold-cracking risk | Increases with plate thickness, official-page wording |
| Carbon, heat analysis max | 0.20% |
| P / S, heat analysis max | 0.020% / 0.010% |
| CEV (EN 10025-6:2019, official wording) | Maxima rise with thickness, starting at 0.72 for plates up to 50 mm. The actual CEV of each heat is printed on the mill certificate |
| Hot forming | Not recommended on EN 10025-6 S890QL, because it can destroy the quenched and tempered properties. Confirm forming limits with the mill |
The official mechanical table on EN 10025-6 S890QL remains ReH 890 / 830 / 830 MPa and Rm 940–1100 / 880–1100 / 880–1100 MPa in the 3–50 / >50–100 / >100–125 mm bands, with 11% minimum elongation and Charpy 30 J minimum at −40 °C, longitudinal. The official mechanical table includes a >100–125 mm row from EN 10025-6:2019. The earlier 2004+A1 edition specified S890 grades only up to 100 mm, so state the edition on the order and confirm the guaranteed value for the actual thickness on the mill certificate. Welding procedure qualification must use the ordered thickness, CEV and toughness quality. EN 10025-6 S890Q is tested at −20 °C and allows higher phosphorus and sulfur maxima; EN 10025-6 S890QL1 is tested at −60 °C. They do not automatically satisfy a specified S890QL order.
Frequently Asked Questions (FAQ)
Is EN 10025-6 S890QL weldable?
Yes, with more care than lower-strength structural steels. The official EN 10025-6 S890QL page requires a WPS following EN 1011-2, low-hydrogen consumables and controlled heat input. The grade name alone does not pre-qualify a welding procedure.
What CEV should be used when welding EN 10025-6 S890QL?
Use the actual CEV printed on the mill certificate. Official wording for EN 10025-6:2019 is that the maxima rise with thickness, starting at 0.72 for plates up to 50 mm.
Can EN 10025-6 S890Q be used where EN 10025-6 S890QL welding and toughness are specified?
No. EN 10025-6 S890Q is impact tested at −20 °C and allows higher phosphorus and sulfur maxima. It does not satisfy a specified S890QL order unless the project documents are revised.
For plate to EN 10025-6 S890QL (1.8983), Please contact Gangsteel with the designation, edition, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our carbon and high-strength steel plate at Gangsteel.