Gangsteel supplies ASTM A514 Grade R steel plate (A514 GR.R, A514 Gr.R) as high-yield-strength quenched and tempered alloy steel plate to ASTM A514/A514M, of structural quality, suitable for welding. Grade R is a nickel-chromium-molybdenum-vanadium grade, with a Table 1 maximum thickness of 2½ in. [65 mm] and a minimum yield strength of 100 ksi [690 MPa] in the official Table 2 bands through 2½ in. [65 mm]. Grade R is a legacy Table 1 grade of ASTM A514/A514M-00a and is not listed in ASTM A514/A514M-22 Table 1. The usual delivery is quenched and tempered, by heating to not less than 1650 °F [900 °C], quenching in water or oil, and tempering at not less than 1150 °F [620 °C]. This is not ASTM A517 pressure-vessel plate. Existing ASTM A514 grade pages on this site include ASTM A514 Grade A, ASTM A514 Grade B, ASTM A514 Grade C, ASTM A514 Grade E, ASTM A514 Grade F, ASTM A514 Grade H, ASTM A514 Grade J, ASTM A514 Grade K, ASTM A514 Grade P, ASTM A514 Grade Q, ASTM A514 Grade S, ASTM A514 Grade T. Within the pressure-vessel and boiler steel plate range, Gangsteel coordinates mill production, plate processing and export supply around the contractual edition and the requirements of each order.

This page is a full-site official-style product-body remediation under the existing parent category pressure-vessel and boiler steel plate. It is not part of the named official-product-standards hubs, and no child ASTM A514 taxonomy is created. ASTM A514/A514M covers high-yield-strength, quenched and tempered alloy steel plate of structural quality, suitable for welding. It is not the pressure-vessel specification ASTM A517/A517M. The held current published edition is ASTM A514/A514M-22. That 22 Table 1 (and the -05 Table 1) lists only Grades A, B, E, F, H, P, Q and S. ASTM A514 Grade R is not listed in the 22 or 05 Table 1. It is listed in official ASTM A514/A514M-00a Table 1. Chemistry and the grade’s maximum thickness on this page are the official 00a Table 1 values, including the 00a phosphorus and sulphur maxima, and are not presented as A514/A514M-22 requirements. The 00a Table 2 tensile bands match the 22 Table 2 specified values for the same thickness rows; this page clips Table 2 to the 00a maximum thickness of Grade R. Whether Grade R can be certified to a current ASTM A514/A514M purchase order is a matter for the contractual edition and the mill; this page does not invent a current-edition Table 1 row for a grade that is not listed there. The contractual edition named on the purchase order, the mill certificate and ASTM A6/A6M govern. No figure from ASTM A517 or from a current-grade A514 Table 1 is presented as a 22 requirement for this legacy grade.

Grade Designation

  • Standard: ASTM A514/A514M-00a Table 1 (Grade R is not in the 22 or 05 Table 1); Table 2 tensile bands from 00a, which match 22, clipped to the 00a maximum thickness.
  • Steel name: ASTM A514 Grade R (also written A514 GR.R, A514 Gr.R, A514GR.R).
  • Status: legacy Table 1 grade of A514/A514M-00a, not listed in A514/A514M-22.
  • Quality: high-yield-strength quenched and tempered alloy steel plate, structural quality, suitable for welding.
  • Usual delivery: quenched and tempered (heating to not less than 1650 °F [900 °C], water or oil quench, tempering at not less than 1150 °F [620 °C]). Plates may be ordered without that heat treatment, in which case the manufacturer stress-relieves and subsequent heat treatment is the purchaser’s responsibility (clause 5.2).
  • Table 1 maximum thickness for Grade R: 2½ in. [65 mm].
  • General requirements: ASTM A6/A6M. The steel shall be killed and shall conform to the fine austenitic grain size requirements of A6/A6M.

Key Advantages of ASTM A514 Grade R Steel Plate

  • Nickel-chromium-molybdenum-vanadium chemistry, with a specified maximum thickness of 2½ in. [65 mm].
  • 100 ksi [690 MPa] minimum yield strength in the official tensile table for plate 2½ in. [65 mm] and under (A514 Table 2) or 2.50 in. [65 mm] and under (A517 Table 2).
  • Official Table 2 Brinell hardness 235–293 HBW may be used instead of tension testing on plates ⅜ in. [10 mm] and under, under the lot rules of clause 7.2.
  • Legacy 00a listing: this page documents the last official Table 1 chemistry for Grade R and does not invent a 22 Table 1 row.
  • Quenched and tempered delivery as specified, suitable for welding when a procedure appropriate to the grade and service is used.

Chemical Composition of ASTM A514 Grade R Steel Plate

Element Heat analysis, %
C 0.15–0.20
Mn 0.85–1.15
P 0.035 max
S 0.035 max
Si 0.20–0.35
Ni 0.90–1.10
Cr 0.35–0.65
Mo 0.15–0.25
V 0.03–0.08

Cast (heat) analysis, official ASTM A514/A514M-00a Table 1. Grade R is not in the 22 Table 1.

Official A514/A514M-00a Table 1 limits. Grade R has no boron requirement in that table. Grade R is not listed in the 22 (or 05) Table 1.

Product analysis, when specified under Supplementary Requirement S2, shall conform to Table 1 subject to the product-analysis tolerances of ASTM A6/A6M. A product-analysis table is not invented here. Where “…” appears in Table 1 there is no requirement; those elements are omitted from this grade’s table. Elements are heat-analysis ranges or maxima as official; they are not all maxima.

Mechanical Properties of ASTM A514 Grade R Steel Plate

Thickness Tensile strength, ksi [MPa] Yield strength min, ksi [MPa] Elongation in 2 in. [50 mm], min, % Reduction of area, min, % Brinell hardness
To ¾ in. [20 mm], incl 110–130 [760–895] 100 [690] 18 40F 235–293 HBW
Over ¾ in. to 2½ in. [20 to 65 mm], incl 110–130 [760–895] 100 [690] 18 40F, 50G —

Official ASTM A514/A514M Table 2, clipped to the Table 1 maximum thickness of Grade R (2½ in. [65 mm]). Yield strength is measured at 0.2 % offset or 0.5 % extension under load (A370). Elongation and reduction of area need not be determined for floor plates. For plates tested in the transverse direction, elongation is reduced by two percentage points and reduction of area by five percentage points (Table 2 footnote C / A6/A6M). F If measured on the A370 Fig. 3 1½-in. [40-mm] wide tension specimen. G If measured on the A370 Fig. 4 ½-in. [12.5-mm] round tension specimen. A dash means no requirement in that cell. For plates ⅜ in. [10 mm] and under, a Brinell hardness test may be used instead of tension testing each plate, under the lot rules of clause 7.2. This Table 2 is not the ASTM A517 Table 2 (which starts at 115–135 ksi tensile).

Delivery Condition, Tests and Heat Treatment

Except as allowed by clause 5.2, ASTM A514 Grade R plates shall be heat treated to conform to Table 2 by heating to not less than 1650 °F [900 °C], quenching in water or oil, and tempering at not less than 1150 °F [620 °C]. The heat-treatment temperatures shall be reported in the test report. Plates ordered without that heat treatment shall be stress relieved by the manufacturer, and subsequent heat treatment is the purchaser’s responsibility (5.2). The steel shall be killed and shall conform to fine austenitic grain size in A6/A6M. Except as allowed by the ⅜ in. hardness option (7.2), one tension test shall be taken from a corner of each plate as heat treated. The manufacturer may re-heat treat plates that fail to meet the mechanical-property requirements; all mechanical-property tests shall then be repeated. If the steel is to be welded, a procedure suitable for the grade and the intended service is presupposed (see A6/A6M Appendix X3). The purchaser specifies the contractual edition, grade, thickness, dimensions and any supplementary requirements.

Available Dimensions of ASTM A514 Grade R Steel Plate

The official maximum thickness for ASTM A514 Grade R is 2½ in. [65 mm]. Width, length and any processing (cutting, bevelling) are as specified on the order and as the mill can produce. Gangsteel does not publish a standing stock list on this page. The purchaser should state the required thickness, dimensions and quantity at enquiry.

Main Applications of ASTM A514 Grade R Steel Plate

ASTM A514 Grade R is specified for welded structures and other non-welded structures that require high-yield-strength quenched and tempered alloy steel plate of structural quality. Typical uses include bridges, building frames, construction and mining equipment, and other welded structural members, where the purchase order names ASTM A514/A514M Grade R and the contractual edition. It is not, by itself, a substitute for ASTM A517 pressure-vessel plate. Because Grade R is not in the current 22 Table 1, availability and certification must be confirmed against the contractual edition. Suitability for a given design code, thickness and welding procedure is a matter for the purchaser’s specification and the mill certificate.

Equivalent Grades of ASTM A514 Grade R Steel Plate

The following existing Gangsteel product pages are corresponding grades that are often discussed alongside ASTM A514 Grade R. Correspondence is not automatic substitution. The purchase order must name the standard, the grade, the edition and the delivery condition.

Standard Grade Qualification
ASTM A514/A514M Grade A, Grade B, Grade C, Grade E, Grade F, Grade H, Grade J, Grade K, Grade P, Grade Q, Grade S, Grade T Other A514 grades on this site. Each has its own Table 1 chemistry and maximum thickness; all current and 00a grades share Table 2 tensile bands, clipped to each grade’s maximum. Not automatic substitutes for Grade R.
EN 10025-6 S690Q, S690QL, S690QL1 European quenched and tempered structural steels in a comparable 690 MPa yield class. Chemistry, impact and delivery rules are those of EN 10025-6, not of ASTM A514. Closely named grades are not automatic substitutes.

Related Products

FAQ about ASTM A514 Grade R Steel Plate

What is ASTM A514 Grade R steel plate?

ASTM A514 Grade R (A514 GR.R, A514 Gr.R) is a high-yield-strength quenched and tempered alloy steel plate of structural quality to ASTM A514/A514M, suitable for welding. It is a nickel-chromium-molybdenum-vanadium grade. Aliases used in enquiries include A514 Grade R, A514GR.R, A514 Gr.R, A514 Gr R, ASTM A514/A514M Grade R. ASTM A514 Grade R is listed in official ASTM A514/A514M-00a Table 1 and is not listed in the 22 or 05 Table 1. Chemistry and maximum thickness on this page are the 00a values, not invented 22 figures.

What is the usual delivery condition of ASTM A514 Grade R?

ASTM A514 Grade R is supplied quenched and tempered: heated to not less than 1650 °F [900 °C], quenched in water or oil, and tempered at not less than 1150 °F [620 °C], unless ordered without that heat treatment under clause 5.2. This is not ASTM A517 pressure-vessel delivery.

What is the chemical composition of ASTM A514 Grade R?

The official heat-analysis limits for ASTM A514 Grade R are given in the chemical-composition table on this page (A514/A514M-00a Table 1; Grade R is not in the 22 Table 1). Product analysis, when specified, follows Table 1 subject to A6/A6M tolerances.

What are the yield, tensile and elongation values of ASTM A514 Grade R?

Official A514 Table 2 gives, through 2½ in. [65 mm], a tensile range of 110–130 ksi [760–895 MPa], a minimum yield of 100 ksi [690 MPa] and a minimum elongation of 18 %. Grade R is limited to 2½ in. [65 mm], so the over-2½ in. Table 2 row does not extend this grade beyond that maximum. These figures are not the ASTM A517 Table 2 values.

What is the maximum thickness of ASTM A514 Grade R?

The official Table 1 maximum thickness for ASTM A514 Grade R is 2½ in. [65 mm]. That maximum is the 00a Table 1 value. This page does not publish a standing stock list.

Is ASTM A514 Grade R a pressure-vessel steel?

No. ASTM A514 Grade R is a structural-quality ASTM A514/A514M plate. ASTM A517/A517M is the pressure-vessel specification and does not list a Grade R. They are not interchangeable.

Is ASTM A514 Grade R still listed in the current ASTM A514/A514M edition?

No. Grade R appears in official A514/A514M-00a Table 1 and is absent from the 05 and 22 Table 1 headings. Certification to a current purchase order depends on the contractual edition and the mill; this page does not invent a 22 Table 1 for Grade R.

How do I enquire for ASTM A514 Grade R steel plate?

Please contact Gangsteel with the grade A514 GR.R (or ASTM A514 Grade R), the contractual edition of ASTM A514/A514M, thickness and dimensions, and any supplementary requirements (product analysis S2, ultrasonic examination, additional thermal simulation of test pieces). Visit Gangsteel or contact Gangsteel to place the enquiry.

For production, processing and export enquiries for ASTM A514 Grade R steel plate, please contact Gangsteel. Visit Gangsteel for the full plate-supply range.

ASTM A514GR.R|A514 Grade R quenched and tempered steel plate