Gangsteel supplies ASTM A514 Grade B steel plate (A514 GR.B, A514 Gr.B) as high-yield-strength quenched and tempered alloy steel plate to ASTM A514/A514M, of structural quality, suitable for welding. Grade B is a chromium-molybdenum-vanadium-titanium-boron grade, with a Table 1 maximum thickness of 1¼ in. [32 mm] and a minimum yield strength of 100 ksi [690 MPa] in the official Table 2 bands through 2½ in. [65 mm]. The usual delivery is quenched and tempered, by heating to not less than 1650 °F [900 °C], quenching in water or oil, and tempering at not less than 1150 °F [620 °C]. This is not ASTM A517 pressure-vessel plate. Existing ASTM A514 grade pages on this site include ASTM A514 Grade A, ASTM A514 Grade C, ASTM A514 Grade E, ASTM A514 Grade F, ASTM A514 Grade H, ASTM A514 Grade J, ASTM A514 Grade K, ASTM A514 Grade P, ASTM A514 Grade Q, ASTM A514 Grade R, ASTM A514 Grade S, ASTM A514 Grade T. Within the pressure-vessel and boiler steel plate range, Gangsteel coordinates mill production, plate processing and export supply around the contractual edition and the requirements of each order. The live page title and slug historically contain the words “Grade A” after the Grade B designation; those protected fields are left unchanged, and this body is for ASTM A514 Grade B.
This page is a full-site official-style product-body remediation under the existing parent category pressure-vessel and boiler steel plate. It is not part of the named official-product-standards hubs, and no child ASTM A514 taxonomy is created. ASTM A514/A514M is the specification for high-yield-strength, quenched and tempered alloy steel plate, suitable for welding, of structural quality, in thicknesses of 6 in. [150 mm] and under (not every grade is available to that maximum; see Table 1). It is not the pressure-vessel specification ASTM A517/A517M. The held current published edition used here is ASTM A514/A514M-22. Cast (heat) analysis, grade maximum thickness, and the current eight-grade Table 1 set (A, B, E, F, H, P, Q, S) follow that 22 Table 1, as recovered from the published -22 sample and the A514/A514M-18ε1 to -22 redline, and cross-checked against official A514/A514M-00a for figures that did not change. Room-temperature tensile, elongation, reduction-of-area and Brinell hardness figures are the official Table 2 specified bands, which are the same in 00a and 22, clipped to this grade’s Table 1 maximum thickness. Relative to 00a, the 22 edition lowered the phosphorus and sulphur maxima for the current grades to 0.030 % (Grade S sulphur remains 0.020 %) and revised some individual ranges (for example Grade B titanium). A later edition, if named on the purchase order, governs. Official 22 Table 1 does not list Grades C, J, K, M, R or T; those letters that have existing Gangsteel pages are remediated from 00a and are not given invented 22 chemistry. There is no ASTM A514 Grade M page on this site and none is invented. ASTM A514 Grade P and ASTM A514 Grade Q are existing already-revised Grade P and Grade Q pages, linked where relevant and not redrafted here. No figure from ASTM A517, ASME SA-517, EN 10025-6 or EN 10028-6 is presented as an ASTM A514 requirement. The contractual edition named on the purchase order, the mill certificate and ASTM A6/A6M govern.
Grade Designation
- Standard: ASTM A514/A514M-22 (current held edition) for Table 1 chemistry and maximum thickness; Table 2 tensile bands, identical in 00a and 22, clipped to this grade’s maximum.
- Steel name: ASTM A514 Grade B (also written A514 GR.B, A514 Gr.B, A514GR.B).
- Status: current Table 1 grade of A514/A514M-22.
- Quality: high-yield-strength quenched and tempered alloy steel plate, structural quality, suitable for welding.
- Usual delivery: quenched and tempered (heating to not less than 1650 °F [900 °C], water or oil quench, tempering at not less than 1150 °F [620 °C]). Plates may be ordered without that heat treatment, in which case the manufacturer stress-relieves and subsequent heat treatment is the purchaser’s responsibility (clause 5.2).
- Table 1 maximum thickness for Grade B: 1¼ in. [32 mm].
- General requirements: ASTM A6/A6M. The steel shall be killed and shall conform to the fine austenitic grain size requirements of A6/A6M.
Key Advantages of ASTM A514 Grade B Steel Plate
- Chromium-molybdenum-vanadium-titanium-boron chemistry, with a specified maximum thickness of 1¼ in. [32 mm].
- 100 ksi [690 MPa] minimum yield strength in the official tensile table for plate 2½ in. [65 mm] and under (A514 Table 2) or 2.50 in. [65 mm] and under (A517 Table 2).
- Official Table 2 Brinell hardness 235–293 HBW may be used instead of tension testing on plates ⅜ in. [10 mm] and under, under the lot rules of clause 7.2.
- Quenched and tempered delivery as specified, suitable for welding when a procedure appropriate to the grade and service is used.
Chemical Composition of ASTM A514 Grade B Steel Plate
| Element | Heat analysis, % |
|---|---|
| C | 0.12–0.21 |
| Mn | 0.70–1.00 |
| P | 0.030 max |
| S | 0.030 max |
| Si | 0.20–0.35 |
| Cr | 0.40–0.65 |
| Mo | 0.15–0.25 |
| V | 0.03–0.08 |
| Ti | 0.01–0.10 |
| B | 0.0005–0.005 |
Cast (heat) analysis, official ASTM A514/A514M-22 Table 1.
The A514/A514M-22 titanium range for Grade B is 0.01–0.10 % (A514/A514M-00a stated 0.01–0.03 %). Vanadium may be substituted for part or all of titanium on a one-for-one basis (Table 1 footnote A).
Product analysis, when specified under Supplementary Requirement S2, shall conform to Table 1 subject to the product-analysis tolerances of ASTM A6/A6M. A product-analysis table is not invented here. Where “…” appears in Table 1 there is no requirement; those elements are omitted from this grade’s table. Elements are heat-analysis ranges or maxima as official; they are not all maxima.
Mechanical Properties of ASTM A514 Grade B Steel Plate
| Thickness | Tensile strength, ksi [MPa] | Yield strength min, ksi [MPa] | Elongation in 2 in. [50 mm], min, % | Reduction of area, min, % | Brinell hardness |
|---|---|---|---|---|---|
| To ¾ in. [20 mm], incl | 110–130 [760–895] | 100 [690] | 18 | 40F | 235–293 HBW |
| Over ¾ in. to 2½ in. [20 to 65 mm], incl | 110–130 [760–895] | 100 [690] | 18 | 40F, 50G | — |
Official ASTM A514/A514M Table 2, clipped to the Table 1 maximum thickness of Grade B (1¼ in. [32 mm]). Yield strength is measured at 0.2 % offset or 0.5 % extension under load (A370). Elongation and reduction of area need not be determined for floor plates. For plates tested in the transverse direction, elongation is reduced by two percentage points and reduction of area by five percentage points (Table 2 footnote C / A6/A6M). F If measured on the A370 Fig. 3 1½-in. [40-mm] wide tension specimen. G If measured on the A370 Fig. 4 ½-in. [12.5-mm] round tension specimen. A dash means no requirement in that cell. For plates ⅜ in. [10 mm] and under, a Brinell hardness test may be used instead of tension testing each plate, under the lot rules of clause 7.2. This Table 2 is not the ASTM A517 Table 2 (which starts at 115–135 ksi tensile).
Delivery Condition, Tests and Heat Treatment
Except as allowed by clause 5.2, ASTM A514 Grade B plates shall be heat treated to conform to Table 2 by heating to not less than 1650 °F [900 °C], quenching in water or oil, and tempering at not less than 1150 °F [620 °C]. The heat-treatment temperatures shall be reported in the test report. Plates ordered without that heat treatment shall be stress relieved by the manufacturer, and subsequent heat treatment is the purchaser’s responsibility (5.2). The steel shall be killed and shall conform to fine austenitic grain size in A6/A6M. Except as allowed by the ⅜ in. hardness option (7.2), one tension test shall be taken from a corner of each plate as heat treated. The manufacturer may re-heat treat plates that fail to meet the mechanical-property requirements; all mechanical-property tests shall then be repeated. If the steel is to be welded, a procedure suitable for the grade and the intended service is presupposed (see A6/A6M Appendix X3). The purchaser specifies the contractual edition, grade, thickness, dimensions and any supplementary requirements.
Available Dimensions of ASTM A514 Grade B Steel Plate
The official maximum thickness for ASTM A514 Grade B is 1¼ in. [32 mm]. Width, length and any processing (cutting, bevelling) are as specified on the order and as the mill can produce. Gangsteel does not publish a standing stock list on this page. The purchaser should state the required thickness, dimensions and quantity at enquiry.
Main Applications of ASTM A514 Grade B Steel Plate
ASTM A514 Grade B is specified for welded structures and other non-welded structures that require high-yield-strength quenched and tempered alloy steel plate of structural quality. Typical uses include bridges, building frames, construction and mining equipment, and other welded structural members, where the purchase order names ASTM A514/A514M Grade B and the contractual edition. It is not, by itself, a substitute for ASTM A517 pressure-vessel plate. Suitability for a given design code, thickness and welding procedure is a matter for the purchaser’s specification and the mill certificate.
Equivalent Grades of ASTM A514 Grade B Steel Plate
The following existing Gangsteel product pages are corresponding grades that are often discussed alongside ASTM A514 Grade B. Correspondence is not automatic substitution. The purchase order must name the standard, the grade, the edition and the delivery condition.
| Standard | Grade | Qualification |
|---|---|---|
| ASTM A514/A514M | Grade A, Grade C, Grade E, Grade F, Grade H, Grade J, Grade K, Grade P, Grade Q, Grade R, Grade S, Grade T | Other A514 grades on this site. Each has its own Table 1 chemistry and maximum thickness; all current and 00a grades share Table 2 tensile bands, clipped to each grade’s maximum. Not automatic substitutes for Grade B. |
| ASTM A517/A517M | ASTM A517 Grade B | Pressure-vessel quenched and tempered plate with a related grade letter. Chemistry is similar but not identical (for example P and S maxima, and some silicon, titanium or molybdenum ranges differ). Tensile Table 2 starts at 115–135 ksi, not the A514 110–130 ksi band, and A517 requires transverse Charpy lateral expansion. Not an automatic substitute. |
| ASME SA-517 | ASME SA517 Grade B | ASME Section II counterpart of ASTM A517 (identical with A517-17 except for a boron footnote). A pressure-vessel specification, not A514. Not an automatic substitute. |
| EN 10025-6 | S690Q, S690QL, S690QL1 | European quenched and tempered structural steels in a comparable 690 MPa yield class. Chemistry, impact and delivery rules are those of EN 10025-6, not of ASTM A514. Closely named grades are not automatic substitutes. |
Related Products
- ASTM A514 Grade A — same specification, different Table 1 grade.
- ASTM A514 Grade C (legacy 00a listing) — same specification, different Table 1 grade.
- ASTM A514 Grade E — same specification, different Table 1 grade.
- ASTM A514 Grade F — same specification, different Table 1 grade.
- ASTM A514 Grade H — same specification, different Table 1 grade.
- ASTM A514 Grade J (legacy 00a listing) — same specification, different Table 1 grade.
- ASTM A514 Grade K (legacy 00a listing) — same specification, different Table 1 grade.
- ASTM A514 Grade P (already revised) — same specification, different Table 1 grade.
- ASTM A514 Grade Q (already revised) — same specification, different Table 1 grade.
- ASTM A514 Grade R (legacy 00a listing) — same specification, different Table 1 grade.
- ASTM A514 Grade S — same specification, different Table 1 grade.
- ASTM A514 Grade T (legacy 00a listing) — same specification, different Table 1 grade.
- ASTM A517 Grade B and ASME SA517 Grade B — corresponding pressure-vessel plates, not automatic substitutes.
- EN 10025-6 S690QL — comparable 690 MPa structural QT steel, different standard.
- Pressure-vessel and boiler steel plate — parent category range.
FAQ about ASTM A514 Grade B Steel Plate
What is ASTM A514 Grade B steel plate?
ASTM A514 Grade B (A514 GR.B, A514 Gr.B) is a high-yield-strength quenched and tempered alloy steel plate of structural quality to ASTM A514/A514M, suitable for welding. It is a chromium-molybdenum-vanadium-titanium-boron grade. Aliases used in enquiries include A514 Grade B, A514GR.B, A514 Gr.B, A514 Gr B, ASTM A514/A514M Grade B. ASTM A514 Grade B is a current Table 1 grade of ASTM A514/A514M-22.
What is the usual delivery condition of ASTM A514 Grade B?
ASTM A514 Grade B is supplied quenched and tempered: heated to not less than 1650 °F [900 °C], quenched in water or oil, and tempered at not less than 1150 °F [620 °C], unless ordered without that heat treatment under clause 5.2. This is not ASTM A517 pressure-vessel delivery.
What is the chemical composition of ASTM A514 Grade B?
The official heat-analysis limits for ASTM A514 Grade B are given in the chemical-composition table on this page (A514/A514M-22 Table 1). Product analysis, when specified, follows Table 1 subject to A6/A6M tolerances.
What are the yield, tensile and elongation values of ASTM A514 Grade B?
Official A514 Table 2 gives, through 2½ in. [65 mm], a tensile range of 110–130 ksi [760–895 MPa], a minimum yield of 100 ksi [690 MPa] and a minimum elongation of 18 %. Grade B is limited to 1¼ in. [32 mm], so the over-2½ in. Table 2 row does not extend this grade beyond that maximum. These figures are not the ASTM A517 Table 2 values.
What is the maximum thickness of ASTM A514 Grade B?
The official Table 1 maximum thickness for ASTM A514 Grade B is 1¼ in. [32 mm]. This page does not publish a standing stock list.
Is ASTM A514 Grade B the same as ASTM A517 Grade B?
No. ASTM A517 Grade B is a pressure-vessel plate with a related letter, different tensile table, tighter P and S maxima, and a mandatory Charpy lateral-expansion requirement. It is not an automatic substitute for ASTM A514 Grade B. The purchase order must name the standard that applies.
Is ASTM A514 Grade B still listed in the current ASTM A514/A514M edition?
Yes. Grade B is one of the eight grades in A514/A514M-22 Table 1 (A, B, E, F, H, P, Q, S).
How do I enquire for ASTM A514 Grade B steel plate?
Please contact Gangsteel with the grade A514 GR.B (or ASTM A514 Grade B), the contractual edition of ASTM A514/A514M, thickness and dimensions, and any supplementary requirements (product analysis S2, ultrasonic examination, additional thermal simulation of test pieces). Visit Gangsteel or contact Gangsteel to place the enquiry.
Why does the ASTM A514 Grade B page title mention Grade A?
The live WordPress title and slug for this page are the historical strings “ASTM A514GR.B|A514 Grade A quenched and tempered steel plate” and “astm-a514gr-b-a514-grade-a-quenched-and-tempered-steel-plate”. Those protected fields are left unchanged. The product specified on this page is ASTM A514 Grade B (A514 GR.B), with Grade B Table 1 chemistry.
For production, processing and export enquiries for ASTM A514 Grade B steel plate, please contact Gangsteel. Visit Gangsteel for the full plate-supply range.