ASTM A516 Grade 60, also commonly written as A516GR.60, A516 Gr.60, A516 GR 60 and ASTM A516/A516M Grade 60 [Grade 415], is the inch-pound Grade 60 designation in ASTM A516/A516M. Grade 415 is the SI designation in the same specification, not a converted Grade 60 value. ASME SA516 Grade 60 (SA-516 or SA-516M Grade 60 or Grade 415) is the corresponding ASME family designation, not merely another spelling of the ASTM name. An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true. The official product page is ASTM A516 Grade 60.

This page states the published tensile, yield and elongation figures for ASTM A516 Grade 60 [Grade 415]. These are the official public-reference mechanical properties already disclosed on ASTM A516 Grade 60 and ASME SA516 Grade 60. They are not a certified extract of every clause in the current ASTM or ASME edition. Inch-pound Grade 60 and SI Grade 415 values are independent and are not converted from one another on this page.

ASTM A516 Grade 60 Mechanical Properties

Property Published reference value Basis / conditions
Tensile strength, Grade 60 60–80 ksi Inch-pound; ASTM A516/A516M-25 public Scope
Tensile strength, Grade 415 415–550 MPa SI; ASTM A516/A516M-25 public Scope. Inch-pound and SI values are independent, not exact conversions
Minimum yield strength 32 ksi Inch-pound; SSAB Grade 60 published required properties, as disclosed on the official ASTM A516 Grade 60 and ASME SA516 Grade 60 pages. 32 ksi is not published here as 220 MPa or as an official SI specification value
Minimum elongation, 2 in. [50 mm] gauge 25% SSAB required properties as used on the official grade page; thickness adjustments per A20/A20M or the corresponding ordered SA-20 requirements
Minimum elongation, 8 in. [200 mm] gauge 21% Same reference basis and applicable thickness adjustments

The 32 ksi yield minimum is a required-property figure from the SSAB Grade 60 datasheet as used on the official pages, not a typical heat result and not an official SI value. Do not treat 32 ksi as 220 MPa for an SI order. Where the purchase order is written to Grade 415, use the SI tensile range from the A516/A516M-25 public Scope and confirm the SI yield in the ordered edition; this page does not invent that SI yield figure.

Elongation is reported on both the 2 in. [50 mm] and 8 in. [200 mm] gauges. Thickness adjustments in A20/A20M, or the corresponding SA-20 requirements, still apply and must be assessed before comparing a test result. A percentage detached from its gauge length is not a complete inspection comparison.

What These Figures Do and Do Not Cover

Topic Position used on this page
Thickness effect on the tensile range The official Grade 60 tensile range is not restated as a thickness-banded strength table. Chemistry carbon maxima are thickness-banded; the tensile and yield figures above are the grade values used on the official pages
Delivery condition Public compilations and the SSAB Grade 60 datasheet indicate normalizing over 1.50 in. [40 mm] unless otherwise ordered, and as-rolled at or below that thickness unless otherwise agreed or unless notch toughness is specified. Normalizing does not rewrite the tensile range
Related A516 grades ASTM A516 Grade 65 is published as 65–85 ksi tensile with a 35 ksi yield minimum; ASTM A516 Grade 70 as 70–90 ksi tensile with a 38 ksi yield minimum. Those are different grades, not Grade 60 values and not replacements for Grade 60
Allowable stress ASTM A516 does not itself publish an allowable design stress. For many ASME Section VIII Division 1 designs, use the applicable ASME Section II-D table for the SA-516 Grade 60 line, not a conversion of these tensile figures
Hardness or impact energy Not part of the basic Grade 60 mechanical table. Charpy testing is supplementary; hardness is not an A516 specified acceptance value

Certification of a plate still depends on the ordered edition, unit system, product analysis where required, and any supplementary tests written on the order.

Frequently Asked Questions (FAQ)

What is the yield strength of ASTM A516 Grade 60?

The official public-reference minimum yield used on ASTM A516 Grade 60 is 32 ksi, from SSAB’s Grade 60 required properties. It is a minimum, not a typical value, and is not published here as 220 MPa.

What is the tensile strength of ASTM A516 Grade 60?

ASTM A516/A516M-25 public Scope gives 60–80 ksi for Grade 60 and 415–550 MPa for Grade 415. The two unit systems are independent.

Does normalizing change the yield strength of ASTM A516 Grade 60?

Normalizing is a delivery condition. It does not replace the Grade 60 tensile and yield table with a different specified range. Any additional requirements belong on the order.

Where are the official ASTM A516 Grade 60 mechanical properties published on this site?

On ASTM A516 Grade 60 and, for the ASME designation, on ASME SA516 Grade 60.

For plate to ASTM A516/A516M Grade 60 [Grade 415] or ASME SA-516 Grade 60, please contact Gangsteel with the designation, edition, unit system, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our pressure-vessel and boiler steel plate at Gangsteel.

A516 Grade 60 Yield Strength and Mechanical Properties