ASTM A516 Grade 60, also commonly written as A516GR.60, A516 Gr.60, A516 GR 60 and ASTM A516/A516M Grade 60 [Grade 415], is the inch-pound Grade 60 designation in ASTM A516/A516M. Grade 415 is the SI designation in the same specification, not a converted Grade 60 value. ASME SA516 Grade 60 (SA-516 or SA-516M Grade 60 or Grade 415) is the corresponding ASME family designation, not merely another spelling of the ASTM name. An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true. The official product page is ASTM A516 Grade 60.
This page explains what ASTM A516 Grade 60 is: a carbon-manganese pressure-vessel plate grade in ASTM A516/A516M, intended for moderate and lower-temperature welded vessels and boilers where improved notch toughness is important. The chemistry, strength and delivery figures below are the official public-reference values already disclosed on ASTM A516 Grade 60 and ASME SA516 Grade 60. They are not a certified extract of every clause in the current edition.
What ASTM A516 Grade 60 Is
| Topic | Position used on this page |
|---|---|
| Specification | ASTM A516/A516M. Grade 60 is the inch-pound designation; Grade 415 is the SI designation in the same specification, not a conversion of Grade 60 |
| Corresponding ASME designation | ASME SA516 Grade 60 (SA-516 or SA-516M Grade 60 or Grade 415). An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true |
| Product form and service | Killed carbon-manganese plate for welded pressure vessels, boilers and related equipment when the project names this grade. It is not a structural A6 product and not a piping forging |
| Related A516 grades | ASTM A516 Grade 65 and ASTM A516 Grade 70 are higher-strength grades in the same specification. They are not replacements for Grade 60 |
Chemical Composition (Public Reference)
The official Grade 60 chemistry table is thickness-banded for carbon and offers a thin-plate manganese choice that is specific to Grade 60. Confirm the ordered edition and whether a product analysis is required.
| Element / condition | Published public-reference limits on ASTM A516 Grade 60 |
|---|---|
| Carbon, max, heat = product | 0.21% at 1/2 in. [12.5 mm] and under; 0.23% over 1/2 to 2 in. [12.5 to 50 mm]; 0.25% over 2 to 4 in. [50 to 100 mm]; 0.27% over 4 to 8 in. [100 to 200 mm]; 0.27% over 8 in. [200 mm] |
| Manganese, 1/2 in. [12.5 mm] and under | A purchaser choice: 0.60–0.90% heat (0.55–0.98% product) or the higher 0.85–1.20% heat (0.79–1.30% product) option |
| Manganese, over 1/2 in. [12.5 mm] | 0.85–1.20% heat, 0.79–1.30% product |
| Carbon–manganese adjustment | For each 0.01% below the specified carbon maximum, manganese may increase 0.06% above the specified manganese maximum, up to 1.50% heat / 1.60% product |
| Silicon | 0.15–0.40% heat, 0.13–0.45% product |
| Phosphorus / sulfur, max | 0.025 or 0.035 each. 0.035 appears in A516/A516M-06 and SA-516 identical compilations; 0.025 appears in PipingMart 2022 and compilations citing A516/A516M-25. This is not a confirmed official current-edition extract. Use the ordered edition |
Mechanical Properties and Delivery Condition
| Property | Published reference value | Basis / conditions |
|---|---|---|
| Tensile strength, Grade 60 | 60–80 ksi | Inch-pound; ASTM A516/A516M-25 public Scope |
| Tensile strength, Grade 415 | 415–550 MPa | SI; ASTM A516/A516M-25 public Scope. Inch-pound and SI values are independent, not exact conversions |
| Minimum yield strength | 32 ksi | Inch-pound; SSAB Grade 60 published required properties, as disclosed on the official ASTM A516 Grade 60 and ASME SA516 Grade 60 pages. 32 ksi is not published here as 220 MPa or as an official SI specification value |
| Minimum elongation, 2 in. [50 mm] gauge | 25% | SSAB required properties as used on the official grade page; thickness adjustments per A20/A20M or the corresponding ordered SA-20 requirements |
| Minimum elongation, 8 in. [200 mm] gauge | 21% | Same reference basis and applicable thickness adjustments |
Public compilations and the SSAB Grade 60 datasheet indicate that plates over 1.50 in. [40 mm] are supplied normalized unless otherwise ordered, while thinner plate is commonly as-rolled unless otherwise agreed or unless notch toughness is specified, in which case normalizing is the usual condition unless the purchaser specifies otherwise. Normalizing does not change the chemistry or tensile tables. Charpy impact testing, HIC/NACE testing and a hardness acceptance value are not automatic A516 Grade 60 requirements; order them if the project needs them.
Allowable design stress is not published in ASTM A516. For many ASME Section VIII Division 1 designs, use the applicable ASME Section II-D table for the SA-516 Grade 60 line.
Frequently Asked Questions (FAQ)
What is ASTM A516 Grade 60 steel plate used for?
It is a killed carbon-manganese pressure-vessel plate grade for moderate and lower-temperature welded vessels and boilers where improved notch toughness is important, when the project specifies ASTM A516 Grade 60 or the corresponding ASME SA-516 Grade 60 designation.
Is Grade 415 the same as ASTM A516 Grade 60?
Grade 415 is the SI designation in ASTM A516/A516M. It is not a converted Grade 60 value. Inch-pound and SI tensile figures are independent; confirm the unit system written on the order.
Is ASME SA516 Grade 60 identical to ASTM A516 Grade 60?
They are corresponding family designations, not interchangeable certificates. Use ASME SA516 Grade 60 when the order is written to the ASME name, and ASTM A516 Grade 60 when it is written to the ASTM name.
Where is the official product page for ASTM A516 Grade 60?
The official product page is ASTM A516 Grade 60. Contact details for an enquiry are given below.
For plate to ASTM A516/A516M Grade 60 [Grade 415] or ASME SA-516 Grade 60, please contact Gangsteel with the designation, edition, unit system, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our pressure-vessel and boiler steel plate at Gangsteel.