ASME SA516 Grade 60, also commonly written as SA516GR.60, SA-516 Grade 60, SA516 GR 60 and ASME SA-516/SA-516M Grade 60 [Grade 415], is the ASME family designation corresponding to ASTM A516/A516M Grade 60 [Grade 415]. Grade 415 is the SI designation in the same family, not a converted Grade 60 value. ASTM A516 Grade 60 is the corresponding ASTM designation, not merely another spelling of the ASME name. An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true. The official product page is ASME SA516 Grade 60.

This page states the published tensile, yield and elongation figures for ASME SA516 Grade 60 [Grade 415]. These are the official public-reference mechanical properties already disclosed on ASME SA516 Grade 60 and ASTM A516 Grade 60. Inch-pound Grade 60 and SI Grade 415 values are independent and are not converted from one another on this page.

ASME SA516 Grade 60 Mechanical Properties

Property Published reference value Basis / conditions
Tensile strength, Grade 60 60–80 ksi Inch-pound; ASTM A516/A516M-25 public Scope, as used on ASTM A516 Grade 60
Tensile strength, Grade 415 415–550 MPa SI; same public Scope. Inch-pound and SI values are independent, not exact conversions
Minimum yield strength 32 ksi Inch-pound; SSAB Grade 60 required properties as used on the official ASTM A516 Grade 60 and ASME SA516 Grade 60 pages. 32 ksi is not published here as 220 MPa or as an official SI specification value
Minimum elongation, 2 in. [50 mm] / 8 in. [200 mm] 25% / 21% SSAB required properties as used on the official pages, with A20/A20M or SA-20 thickness adjustments

The 32 ksi yield minimum is a required-property figure from the SSAB Grade 60 datasheet as used on the official pages, not a typical heat result and not an official SI value. Elongation percentages are gauge-length minima, not thickness bands; A20/A20M or SA-20 adjustments still apply. Normalizing does not rewrite the tensile range. Allowable design stress is not published in A516 or SA-516; for many ASME VIII-1 designs, use the applicable II-D table for the SA-516 Grade 60 line.

ASME SA516 Grade 65 and ASTM A516 Grade 70 are different strength grades, not Grade 60 values.

Frequently Asked Questions (FAQ)

What is the yield strength of ASME SA516 Grade 60?

The official public-reference minimum yield used on ASME SA516 Grade 60 is 32 ksi, from SSAB’s Grade 60 required properties. It is a minimum, not a typical value, and is not published here as 220 MPa.

What is the tensile strength of ASME SA516 Grade 60?

The A516/A516M-25 public Scope, as used on the official family pages, gives 60–80 ksi for Grade 60 and 415–550 MPa for Grade 415. The two unit systems are independent.

Does normalizing change the mechanical properties of ASME SA516 Grade 60?

Normalizing is a delivery condition. It does not replace the Grade 60 tensile and yield table with a different specified range.

Where are the official ASME SA516 Grade 60 mechanical properties published on this site?

On ASME SA516 Grade 60 and ASTM A516 Grade 60.

For plate to ASTM A516/A516M Grade 60 [Grade 415] or ASME SA-516 Grade 60, please contact Gangsteel with the designation, edition, unit system, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our pressure-vessel and boiler steel plate at Gangsteel.