EN 10025-6 S690QL1, also written S690 QL1, EN10025-6 S690QL1 and steel number 1.8988, is a quenched and tempered structural steel. EN 10025-6 and the official EN 10025-6 S690QL1 page do not specify a hardness requirement. This page therefore records the official tensile range and supplies only a labeled conventional conversion so the hardness title is not left unanswered.

EN 10025-6 S690QL1 Hardness — Specified Versus Conventional

Item Value Basis / conditions
Specified hardness Not specified No hardness table on EN 10025-6 or on EN 10025-6 S690QL1
Official Rm, 3–50 mm 770–940 MPa Official mechanical table
Official Rm, >50–100 mm 760–930 MPa Official mechanical table
Official Rm, >100–150 mm 710–900 MPa Official mechanical table, 2004+A1 thickness steps
Conventional approximate HBW, 3–50 mm About 220–270 HBW Orientation only: HBW ≈ Rm (MPa) / 3.5 from 770–940 MPa. Not a specified limit and not a mill-certificate default
Conventional approximate HBW, >50–100 mm About 215–265 HBW Same conversion from 760–930 MPa, same limitation

The conversion uses a familiar structural-steel approximation and is not taken from an EN 10025-6 hardness table. Do not use it as a production limit, an acceptance criterion, or a substitute for the specified yield, tensile or Charpy tests. Official yield values remain 690 / 650 / 630 MPa in the 3–50 / >50–100 / >100–150 mm bands, with 14% minimum elongation and a −60 °C QL1-quality impact test.

Frequently Asked Questions (FAQ)

What hardness is specified for EN 10025-6 S690QL1?

None. EN 10025-6 S690QL1 publishes yield, tensile, elongation and impact values, not a hardness requirement.

What conventional hardness range is sometimes quoted for EN 10025-6 S690QL1?

Converting the official 770–940 MPa tensile range with HBW ≈ Rm / 3.5 gives about 220–270 HBW for the 3–50 mm band. That figure is an orientation only, not a specified hardness.

Can hardness replace the impact test for EN 10025-6 S690QL1?

No. The official QL1-quality requirement is Charpy testing at −60 °C, with a 30 J longitudinal minimum at that temperature. Hardness is not a substitute for that test.

For plate to EN 10025-6 S690QL1 (1.8988), Please contact Gangsteel with the designation, edition, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our carbon and high-strength steel plate at Gangsteel.

EN 10025-6 S690QL1 Hardness