Gangsteel supplies KR Grade DH32 (R/D32) shipbuilding steel plate against the Korean Register Part 2, Chapter 1, Section 3 hull-structural grade identified below, the contract edition and the issued certificate.
Numerical requirements on this page are transcribed from the official Korean Register, Rules for the Classification of Steel Ships, Part 2 Materials and Welding, 2026, English edition (RA-02-E KR), Chapter 1, Section 3, 301. Rolled steels for hull structural, including Tables 2.1.5, 2.1.6 (marked 2021), 2.1.7 (marked 2021) and 2.1.9, together with Chapter 1, 103 (chemical composition) and 301.7 (test specimens). Unless expressly specified otherwise, those Rules apply to ships or offshore units contracted for construction on or after 1 July 2026, or when the application for certification of materials and welding is dated on or after 1 July 2026. The 2026 front-matter amendments to the 2025 edition do not amend Section 3 hull-steel Tables 2.1.6 and 2.1.7. The figures below are 2026 KR rule requirements for plate, not measured results for a particular heat. The edition named in the contract, the certificate and the attending surveyor govern any actual supply.
Grade Designation
Table 2.1.5 classifies this higher-strength hull steel as DH 32 (also written DH32 in Table 2.1.7). Commercial and documentation forms include KR Grade DH32 and R/D32, as on this official product page. It is one of three higher-strength levels (315, 355 and 390 N/mm²), each with four toughness grades based on the impact-test temperature (Table 2.1.5, note 2).
Key Advantages of DH32 Steel Plate
KR Grade DH32 (R/D32) is a weldable higher-strength hull structural steel in 2026 KR Part 2, Chapter 1, Section 3, Table 2.1.7 (minimum yield 315 N/mm²), with a −20 °C Charpy V-notch laboratory test class. It is used for welded ship structural members where this KR grade is specified.
Chemical Composition (Ladle Analysis)
Table 2.1.6, ladle analysis (Ch 1, 103.1).
| Element / requirement | Value | Notes |
|---|---|---|
| Deoxidation | Killed and fine grain treated | Table 2.1.6, all higher-strength grades, t ≤ 100 mm. |
| C, max. (%) | 0.18 | — |
| Mn (%) | 0.90–1.60 | For steels up to 12.5 mm inclusive, the minimum manganese content may be reduced to 0.70 % (Table 2.1.6, note 7). |
| Si, max. (%) | 0.50 | — |
| P, max. (%) | 0.035 | — |
| S, max. (%) | 0.035 | — |
| Al (acid soluble), min. (%) | 0.015 | May be determined as total aluminium, which is then not to be less than 0.020 % (note 8). The steel is to contain Al, Nb, V or other suitable grain-refining elements, singly or in combination; minima apply when used singly, and not when used in combination (note 10). |
| Nb (%) | 0.02–0.05 | When used singly (note 10). Total Nb + V + Ti is to be less than 0.12 % (note 11). |
| V (%) | 0.05–0.10 | When used singly (note 10). Total Nb + V + Ti is to be less than 0.12 % (note 11). |
| Ti, max. (%) | 0.02 | Included in the note 11 total (less than 0.12 %). |
| Cu, max. (%) | 0.35 | Table 2.1.6; cell shared by A/D/E and F higher-strength grades. |
| Cr, max. (%) | 0.20 | — |
| Ni, max. (%) | 0.40 | — |
| Mo, max. (%) | 0.08 | — |
| N, max. (%) | — | Not specified for A, D and E higher-strength grades in Table 2.1.6. |
| Nb + V + Ti | less than 0.12 % | Table 2.1.6, note 11. |
Ladle analysis of samples from each ladle of each cast (Ch 1, 103.1). Product analysis may be required where the final product chemistry is not well represented by the cast analysis (103.3). For plates and wide flats over 50 mm, and when TMCP is used, slight deviations in chemical composition may be allowed as approved by the Society (301.3 (2)). Other process additions are to be indicated on the test certificate (Table 2.1.6, note 5). For TMCP steels, Ceq and/or Pcm are left to the discretion of the Society (Table 2.1.6, note 13); no numeric Ceq grid is given in Table 2.1.6, and none is invented here.
Mechanical Properties
Tensile specimens: longitudinal axis normal to the final rolling direction, except for sections, bars and flat bars not exceeding 600 mm in width, which are taken parallel (301.7 (2)). Impact specimens are generally taken parallel to the rolling direction (L); transverse (T) when the Society deems it necessary (301.7 (3)). Impact temperatures are laboratory conditions, not approved minimum service temperatures. The table is a rule requirement, not a certificate already issued for a particular plate.
| Property | Requirement | Notes |
|---|---|---|
| Yield strength, min. | 315 N/mm² | Table 2.1.7. |
| Tensile strength | 440–570 N/mm² | Table 2.1.7. |
| Elongation (L = 5.65 √A), min. | 22 % | Table 2.1.7 also gives elongation for R 1B specimens (L = 200 mm) by thickness (note 6). |
| Impact test temperature | −20 °C | Laboratory test condition only, not an approved minimum service temperature. |
| Average absorbed energy, t ≤ 50 mm, L / T, min. | 31 J / 22 J | Table 2.1.7. |
| Average absorbed energy, 50 mm < t ≤ 70 mm, L / T, min. | 38 J / 26 J | Table 2.1.7. |
| Average absorbed energy, 70 mm < t ≤ 100 mm, L / T, min. | 46 J / 31 J | Table 2.1.7. The 2026 KR thickness scope for these plates is t ≤ 100 mm (Table 2.1.5). |
A set fails if two or more specimens are below the specified average, or if a single specimen is below 70 % of that average (Table 2.1.7, note 1). Delivery condition: Table 2.1.9 (DH 32 and DH 36, killed and fine-grain treated): depending on grain-refining practice, product form and thickness up to 100 mm, supply may be as-rolled, ARS or CRS (special approval), controlled-rolled, normalised or TMCP, with the lot sizes in that table. The contractual table governs.
Available Dimensions
Table 2.1.5 applies to higher-strength plates (including flat bars not less than 600 mm wide) up to 100 mm thick, and to sections and bars up to 50 mm thick. Requirements for greater thickness are left to the Society (301.1 (4)). The minus tolerance on nominal thickness is 0.3 mm, irrespective of nominal thickness (301.8 (3) (b)). Width, length and any stock programme are as agreed for the order; no stock size is implied here.
Main Applications
KR Grade DH32 (R/D32) is used for welded hull and ship structural members specified to this Korean Register grade. Fitness for a given location, thickness and service is set by the contract design and the attending society.
Equivalent Grades of DH32
Official comparable product pages, where inventoried, are linked below.
| Society / standard | Comparable grade | Qualification |
|---|---|---|
| ABS | ABS Grade DH32 | Comparison at the same strength and toughness class only. |
| CCS | CCS Grade DH32 | Comparison at the same strength and toughness class only. |
| DNV | DNV Grade DH32 (NV D32) | Comparison at the same strength and toughness class only. |
| GL | GL Grade DH32 | Comparison at the same strength and toughness class only. |
| LR | LR Grade DH32 | Comparison at the same strength and toughness class only. |
Comparison only: not automatic equivalence or substitution. Linked pages state that society’s own requirements, which are not Korean Register requirements. The 2026 KR tables on this page are the only KR numerical source used here. No official gangsteel.com product page is inventoried for BV Grade DH32, and none is invented here.
Related Products
Further official Korean Register hull-steel pages from Gangsteel:
- Korean Register of Shipping shipbuilding steel plates
- KR Grade AH32 (R/A32) steel plate
- KR Grade AH36 (R/A36) steel plate
- KR Grade DH36 (R/D36) steel plate
- KR Grade EH32 (R/E32) steel plate
- KR Grade EH36 (R/E36) steel plate
- KR Grade FH32 (R/F32) steel plate
- KR Grade FH36 (R/F36) steel plate
Frequently Asked Questions (FAQ)
What is KR Grade DH32 (R/D32) steel plate?
KR Grade DH32 (R/D32) is a Korean Register higher-strength hull structural steel in Part 2, Chapter 1, Section 3 of the 2026 KR Rules. The Table 2.1.7 designation is DH32. It has a minimum yield of 315 N/mm² and a −20 °C laboratory impact class.
Does the impact-test temperature define the service limit of KR Grade DH32 (R/D32)?
No. The −20 °C Charpy temperature is a laboratory test condition. Approved service temperature and structural use are set by the ship rules, the design and the attending surveyor.
Can another society’s similarly named grade replace KR Grade DH32 (R/D32) automatically?
No. The Equivalent Grades table is a comparison at the same strength and toughness class, not automatic equivalence or substitution.
Does KR Grade DH32 (R/D32) automatically include through-thickness (Z) properties?
No. Improved through-thickness properties apply only when specified for plates and wide flats 15 mm and over, and are tested under 301.1 (5) and 310. They are not implied by the grade name and are not in these official product titles.
What should an enquiry for KR Grade DH32 (R/D32) include?
State KR Grade DH32 (DH32, R/D32), the governing rules edition, dimensions, quantity, delivery condition, inspection documents, and any transverse impact or through-thickness testing required. Availability is confirmed for the enquiry; none is implied here.