EN 10025-6, also written EN10025-6 and EN 10025-6:2019 (or the earlier EN 10025-6:2004+A1 edition), is the European standard for hot-rolled structural steel plate in the quenched and tempered (Q) condition. The grade names combine a nominal yield class (S460 to S960) with a toughness quality: Q (impact at −20 °C), QL (−40 °C) or QL1 (−60 °C). These are high-strength structural plates, not pressure-vessel designations.
The official product pages used here include EN 10025-6 S460Q, EN 10025-6 S500Q, EN 10025-6 S550Q and EN 10025-6 S690Q, together with the matching QL qualities where linked below. Values are the official public-reference tables already disclosed on those pages. Thickness rows follow the EN 10025-6:2004+A1 steps used on those pages; the 2019 edition revised some thicker-plate steps, so the ordered edition must be stated.
EN 10025-6 High Strength Steel Grades
| Grade (Q quality) | Steel number | ReH min, MPa (3–50 / >50–100 / >100–150 mm) | Rm, MPa (3–50 mm) | Impact, Q quality |
|---|---|---|---|---|
| EN 10025-6 S460Q | 1.8908 | 460 / 440 / 400 | 550–720 | −20 °C, 30 J long. min |
| EN 10025-6 S500Q | 1.8924 | 500 / 480 / 440 | 590–770 | −20 °C, 30 J long. min |
| EN 10025-6 S550Q | 1.8904 | 550 / 530 / 490 | 640–820 | −20 °C, 30 J long. min |
| EN 10025-6 S690Q | 1.8931 | 690 / 650 / 630 | 770–940 | −20 °C, 30 J long. min |
QL and QL1 keep the same strength table as the matching Q grade and change the guaranteed impact temperature to −40 °C or −60 °C. They also use lower phosphorus and sulfur maxima than the Q quality. Official examples at the 500 MPa class are EN 10025-6 S500QL (1.8909) and EN 10025-6 S500QL1 (1.8984). The standard also specifies S620, S890 and S960 classes; those names are not linked here unless an official product page is used.
The steel is fully killed and fine-grained and is delivered quenched and tempered. EN 10025-6 sets maximum CEV values that rise with thickness, up to 0.70 for the thickest plates; the actual CEV of each heat is printed on the mill certificate. Welding should follow a qualified procedure (commonly EN 1011-2). Hot forming is not recommended because it can destroy the quenched and tempered properties.
Frequently Asked Questions (FAQ)
What does the Q, QL or QL1 suffix mean in EN 10025-6?
Q, QL and QL1 are toughness qualities in EN 10025-6, not different strength grades. Q is impact tested at −20 °C, QL at −40 °C and QL1 at −60 °C. A QL or QL1 plate is often reviewed where a Q plate is specified, if the project accepts the colder test; the reverse is not automatic.
Is EN 10025-6 a pressure-vessel specification?
No. EN 10025-6 covers quenched and tempered structural steel. High-temperature pressure-vessel carbon steels are specified in other standards, such as EN 10028-2, and must be named separately when that service is required.
Does the yield strength of an EN 10025-6 grade stay constant with thickness?
No. The official tables reduce the minimum yield in the thicker bands. For EN 10025-6 S500Q, the minima are 500 MPa at 3–50 mm, 480 MPa above 50–100 mm and 440 MPa above 100–150 mm in the 2004+A1 thickness steps used on the official page.
For plate to EN 10025-6 quenched and tempered grades, Please contact Gangsteel with the designation, edition, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our carbon and high-strength steel plate at Gangsteel.