EN 10025-6 S620Q, also written S620 Q, EN10025-6 S620Q and steel number 1.8914, is a quenched and tempered structural steel. EN 10025-6 and the official EN 10025-6 S620Q page do not specify a hardness requirement. This page therefore records the official tensile range and supplies only a labeled conventional conversion so the hardness title is not left unanswered.
EN 10025-6 S620Q Hardness — Specified Versus Conventional
| Item | Value | Basis / conditions |
|---|---|---|
| Specified hardness | Not specified | No hardness table on EN 10025-6 or on EN 10025-6 S620Q |
| Official Rm, 3–50 and >50–100 mm | 700–890 MPa | Official mechanical table |
| Official Rm, >100–150 mm | 650–830 MPa | Official mechanical table, 2004+A1 thickness steps |
| Conventional approximate HBW, 3–100 mm | About 200–255 HBW | Orientation only: HBW ≈ Rm (MPa) / 3.5 from 700–890 MPa. Not a specified limit and not a mill-certificate default |
| Conventional approximate HBW, >100–150 mm | About 185–235 HBW | Same conversion from 650–830 MPa, same limitation |
The conversion uses a familiar structural-steel approximation and is not taken from an EN 10025-6 hardness table. Do not use it as a production limit, an acceptance criterion, or a substitute for the specified yield, tensile or Charpy tests. Official yield values remain 620 / 580 / 560 MPa in the 3–50 / >50–100 / >100–150 mm bands, with 15% minimum elongation and a −20 °C Q-quality impact test.
Frequently Asked Questions (FAQ)
What hardness is specified for EN 10025-6 S620Q?
None. EN 10025-6 S620Q publishes yield, tensile, elongation and impact values, not a hardness requirement.
What conventional hardness range is sometimes quoted for EN 10025-6 S620Q?
Converting the official 700–890 MPa tensile range with HBW ≈ Rm / 3.5 gives about 200–255 HBW for the 3–100 mm bands. That figure is an orientation only, not a specified hardness.
Can hardness replace the impact test for EN 10025-6 S620Q?
No. The official Q-quality requirement is Charpy testing at −20 °C, with a 30 J longitudinal minimum at that temperature. Hardness is not a substitute for that test.
For plate to EN 10025-6 S620Q (1.8914), Please contact Gangsteel with the designation, edition, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our carbon and high-strength steel plate at Gangsteel.