ASTM A516 Grade 60, also commonly written as A516GR.60, A516 Gr.60, A516 GR 60 and ASTM A516/A516M Grade 60 [Grade 415], is the inch-pound Grade 60 designation in ASTM A516/A516M. Grade 415 is the SI designation in the same specification, not a converted Grade 60 value. ASME SA516 Grade 60 (SA-516 or SA-516M Grade 60 or Grade 415) is the corresponding ASME family designation, not merely another spelling of the ASTM name. An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true. The official product page is ASTM A516 Grade 60.
This page compares ASTM A516 Grade 60 with ASTM A36/A36M carbon structural steel. A36 is written to ASTM A6/A6M general requirements for structural products, not to A20/A20M pressure-vessel-plate requirements. Gangsteel does not have an official A36 product page, so the A36 figures below are taken from public compilations of ASTM A36/A36M-19 for plate and are listed without a link. The comparison is not a substitution approval.
Pressure-Vessel Plate versus Carbon Structural Steel
| Topic | ASTM A516 Grade 60 | ASTM A36 / A36M plate |
|---|---|---|
| Type of specification | Pressure-vessel carbon-manganese plate for moderate and lower-temperature service where notch toughness matters, with ASME SA516 Grade 60 as the corresponding ASME designation | Carbon structural steel for riveted, bolted or welded construction of bridges, buildings and general structural purposes |
| General requirements | A20/A20M (or SA-20) | A6/A6M |
| Notch toughness | The specification is written for service where improved notch toughness is important; a Charpy test still has to be ordered if it is required | Not a basic A36 requirement. Any impact test is a supplementary or project requirement |
Chemical Composition of Plate
Grade 60 chemistry is the official public-reference table already disclosed on ASTM A516 Grade 60. A36 plate chemistry is thickness-dependent in A36/A36M-19 compilations (American Alloy Steel and MetalMate). Heat analysis is shown. Copper is only a minimum when copper steel is specified.
| Element / thickness | ASTM A516 Grade 60 [Grade 415], public reference | A36/A36M-19 plate compilations |
|---|---|---|
| Carbon, max | 0.21 / 0.23 / 0.25 / 0.27 by A516 thickness bands (heat = product) | 0.25% to 1½ in. [40 mm]; 0.26% over 1½ to 2½ in.; 0.27% over 2½ to 4 in.; 0.29% over 4 in. |
| Manganese | Grade 60 thickness- and option-dependent ranges, including a thin-plate choice (see the official page) | No specified range to ¾ in. [20 mm]; 0.80–1.20% over ¾ to 2½ in.; 0.85–1.20% over 2½ in. A carbon–manganese allowance to 1.35% Mn is compiled for reductions below the carbon maximum |
| Phosphorus / sulfur, max | 0.025 or 0.035 each; see the official-page source note | 0.030% P and 0.030% S for plate in these compilations |
| Silicon | 0.15–0.40% heat, 0.13–0.45% product | 0.40% max to 1½ in.; 0.15–0.40% over 1½ in. |
| Copper | Not a single named official Grade 60 limit on the pages used here | 0.20% min only when copper steel is specified |
Mechanical Properties
| Property | ASTM A516 Grade 60 [Grade 415] | A36/A36M-19 plate compilations |
|---|---|---|
| Tensile strength | 60–80 ksi / 415–550 MPa, ASTM A516/A516M-25 public Scope | 58–80 ksi [400–550 MPa] for plates, shapes and bars generally |
| Minimum yield strength | 32 ksi, SSAB Grade 60 required properties as used on the official pages. Not published here as 220 MPa or as an official SI specification value | 36 ksi [250 MPa] generally; compilations give 32 ksi [220 MPa] for plate over 8 in. [200 mm] thick |
| Minimum elongation, plates and bars | 25% in 2 in. [50 mm] and 21% in 8 in. [200 mm], with A20/A20M or SA-20 adjustments | 23% in 2 in. [50 mm] and 20% in 8 in. [200 mm], with A6/A6M adjustments (including a two-percentage-point reduction for plates wider than 24 in. [600 mm]) |
A higher A36 yield minimum does not make A36 a pressure-vessel substitute for ASTM A516 Grade 60, and an overlapping tensile range is not identity. ASTM A516 Grade 65 and ASTM A516 Grade 70 are different A516 strength grades, not A36 equivalents. Substitutions require design and project approval.
Frequently Asked Questions (FAQ)
Can ASTM A36 replace ASTM A516 Grade 60?
Not without the project’s design and material approval. ASTM A36 is a structural specification. ASTM A516 Grade 60 is a pressure-vessel plate grade. This comparison is not a substitution approval.
Is ASTM A36 stronger than ASTM A516 Grade 60 because its yield is 36 ksi?
The compiled A36 plate yield minimum is 36 ksi, against a 32 ksi Grade 60 minimum on the official pages. Tensile ranges overlap but are not the same, and the specifications, general-requirements basis and intended use still differ. A single yield figure is not permission to substitute ASTM A516 Grade 60.
Does ASTM A36 have the same toughness rules as ASTM A516 Grade 60?
No. A516 is written for moderate and lower-temperature vessel service where notch toughness matters, but a Charpy test is still ordered only when required. A36 does not, by itself, impose a Charpy test.
Where is the official product page after reading this ASTM A516 Grade 60 and A36 comparison?
Start with ASTM A516 Grade 60. Use ASME SA516 Grade 60 when the order is written to the ASME designation.
For plate to ASTM A516/A516M Grade 60 [Grade 415] or ASME SA-516 Grade 60, please contact Gangsteel with the designation, edition, unit system, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our pressure-vessel and boiler steel plate at Gangsteel.