ASTM A516 Grade 65, also commonly written as A516GR.65, A516 Gr.65, A516 GR 65 and ASTM A516/A516M Grade 65 [Grade 450], is the inch-pound Grade 65 designation in ASTM A516/A516M. Grade 450 is the SI designation in the same specification, not a converted Grade 65 value. ASME SA516 Grade 65 (SA-516 or SA-516M Grade 65 or Grade 450) is the corresponding ASME family designation, not merely another spelling of the ASTM name. An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true. The official product page is ASTM A516 Grade 65.
This page states the public-reference chemical composition of ASTM A516 Grade 65 [Grade 450], already disclosed on ASTM A516 Grade 65 and ASME SA516 Grade 65. The table is a public reference, not a certified extract of every clause in the current ASTM or ASME edition. Acceptance is against the designation, edition and unit system named on the purchase order.
ASTM A516 Grade 65 Chemical Composition
| Element / condition | Heat analysis | Product analysis |
|---|---|---|
| Carbon, max, ½ in. [12.5 mm] and under | 0.24% | 0.24% |
| Carbon, max, over ½ in. to 2 in. [12.5 to 50 mm], incl. | 0.26% | 0.26% |
| Carbon, max, over 2 in. to 4 in. [50 to 100 mm], incl. | 0.28% | 0.28% |
| Carbon, max, over 4 to 8 in. [100 to 200 mm], incl. | 0.29% | 0.29% |
| Carbon, max, over 8 in. [200 mm] | 0.29% | 0.29% |
| Manganese | 0.85–1.20% | 0.79–1.30% |
| Silicon | 0.15–0.40% | 0.13–0.45% |
| Phosphorus / sulfur, max | 0.025 or 0.035 each, heat = product. 0.035 appears in A516/A516M-06 and SA-516 identical compilations; 0.025 appears in PipingMart 2022 and compilations citing A516/A516M-25. This is not a confirmed official current-edition extract. Use the ordered edition | |
Unlike ASTM A516 Grade 60, Grade 65 uses the same manganese range in both the ½ in. and under band and the over ½ in. band. There is no Grade 60-style thin-plate manganese choice on the official Grade 65 table. Do not mix the inch-pound and SI thickness boundaries when classifying a plate at ½ in. / 12.5 mm. The 50 mm carbon step is not the same boundary as the 1.50 in. [40 mm] normalizing threshold.
For each 0.01 percentage point below the specified carbon maximum for that thickness, manganese may increase 0.06 percentage point above the specified manganese maximum, up to 1.50% by heat analysis and 1.60% by product analysis. SSAB’s Grade 65 mill heat analysis (including P 0.020% and S 0.010%) is a producer control, more restrictive than A516 on phosphorus and sulfur, and is not the specification table.
ASTM A516 Grade 60 and ASTM A516 Grade 70 have different carbon maxima and must not be used as the Grade 65 chemistry table.
Frequently Asked Questions (FAQ)
What is the chemical composition of ASTM A516 Grade 65?
Carbon maxima are 0.24 / 0.26 / 0.28 / 0.29 / 0.29% by the official thickness bands, the same for heat and product analysis. Manganese is 0.85–1.20% heat and 0.79–1.30% product in both thickness bands. Silicon is 0.15–0.40% heat and 0.13–0.45% product. Phosphorus and sulfur are 0.025 or 0.035 in public references; use the ordered edition.
Is the manganese range of ASTM A516 Grade 65 the same as Grade 60?
The over-½ in. manganese range is the same style, but ASTM A516 Grade 65 does not have the Grade 60 thin-plate manganese choice. Use the Grade 65 official table, not a Grade 60 table with the number changed.
Does a product analysis of ASTM A516 Grade 65 use the heat-analysis manganese limits?
No. Product-analysis manganese and silicon use the wider ranges in the table. Carbon, phosphorus and sulfur maxima are the same on both bases in the public-reference table used here.
Where is the official ASTM A516 Grade 65 chemistry table on this site?
On ASTM A516 Grade 65 and ASME SA516 Grade 65.
For plate to ASTM A516/A516M Grade 65 [Grade 450] or ASME SA-516 Grade 65, please contact Gangsteel with the designation, edition, unit system, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our pressure-vessel and boiler steel plate at Gangsteel.