EN10025-5 S355J2W steel plate atmospheric corrosion resistance supplier
Gangsteel produced and exported EN10025-5 S355J2W steel plate atmospheric corrosion resistance.We sell EN 10025-5 S355J2W weathering resistance steel plate
Adopt
Standard: BS EN10025-5
Gangsteel keywords: EN10025-5
S355J2W Equivalent, EN10025-5 S355J2W Composition, EN10025-5 S355J2W Properties, EN10025-5 S355J2W density
S355J2W steel plate atmospheric corrosion resistance
S355J2W steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.
S mean S355J2W grade could be used in structural steel projects, 235 is the min yield strength.
J0 ,J2 and K2 standard for the impact degree and energy in 0 temperature.
W means that the mainly different in their carbon and phosphorus contents and availability.
For the steel grade in S235 a maximum carbon equivalent value of 0.44% and for grade s355 a maximum carbon equivalent value of 0.52% based on the ladle analysis shall for all thickness.
Gangsteel
is specialized in improved atmospheric corrosion resistance steel grade. We
exported the grade Corten A and Corten B, 09CuPCrNi-A,09CuPCrNi-B grade,
05CuPCrNi-A steel, and A588 Grade K, A588 Grade A steel.
EN10025-5 S355J2W Chemical composition in Product analysis
Carbon, % | Manganese, % | Cr % | Silicon % | N % max | Sulfur % | |
Max 0.19 | 0.45-1.60 | 0.35-0.85 | Max 0.55 | …. | Max 0.035 | |
Cu % | Phosphorus % | N % | ||||
0.20-0.60 | Max 0.035 | 0.010 |
EN10025-5 S355J2W Mechanical Properties
Grade | Min. Yield Strength Mpa | Tensile Strength MPa | Impact | ||||||||
S355J2W | Nominal Thickness (mm) | Nominal Thickness (mm) | degree | J | |||||||
Thick mm | ≤16 | >16 ≤40 | >40 ≤63 | >63 ≤80 | >80 ≤100 | >100 ≤150 | ≤3 | >3 ≤100 | >100 ≤150 | -20 | 27 |
S355J2W | 355 | 345 | 335 | 325 | 315 | 295 | 510-680 | 470-630 | 450-600 |
If you need in EN10025-5
S355J2W steel plate atmospheric corrosion resistance,
please feel free to contact us by email or calling to us.