CCS GRADE AH32 and CCS/AH32 steel plate supplier
Gangsteel export CCS GRADE AH32 and CCS/AH32 steel plate.CCS Grade AH32 is shipbuilding steel Grade Stock.What are CCS/AH32 shipbuilding steel equal grade?
Keywords: CCS/AH32 Steel plate, CCS Grade AH32, CCS Grade AH32 steel properties, CCS Grade AH32 equivalent material, CCS Grade AH32 round bar, CCS Grade AH32 steel density
Henan Gang iron and steel co., Ltd supply steel grade CCS AH32, CCS DH36, CCS EH36, CCS FH36, CCS AH32, CCS DH32, CCS EH32, CCS FH32, CCS GRADE A, CCS GRADE B, CCS GRADE D, CCS GRADE E. CCS AH40, CCS DH40, CCS EH40, CCS FH40.
AH32 must normalize in each thickness compare with Grade D. For example A, B, D, and E are the ordinary strength in Classification Society.
AH32 steel plate usual be used in the main structural build including the bull and oil platform.
Our mill could produce size in the following:
Thickness: 6mm to 220mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
Henan Gang iron and steel co., Ltd also could supply super thick steel plate thickness from 100mm to 220mm which beyond nine classification society approval.
Henan Gang iron and steel co., Ltd has two large warehouse stock in shanghai port and tianjin port, we have stock in AH32, DH36, EH36, grade D , grade E and steel Coil in Grade A, grade B from thickness 5mm to 18mm in various specification and Classification Society.
If you want order news goods from mill, we could give our mill competitive price for our long business in steel plates. We sincerely hope old and new customers to visit our mill for a long steel business
About AH32 detail information,please refer to technical date in following.
CCS GRADE AH32 and CCS/AH32 steel plate Chemical composition of product analysis:
Grade | C % | Si % | Mn % | P % | S % |
AH32 | 0.180 | 0.10-0.35 | 0.700 | 0.035 | 0.035 |
CCS GRADE AH32 and CCS/AH32 steel plate mechanical properties
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) | Min Impact Energy | |
AH32 | 8mm-50mm | Min 315Mpa | 440-590Mpa | 22% | 0 | 34J |
51mm-70mm | Min 315Mpa | 440-590Mpa | 22% | 0 | 38J | |
71mm-100mm | Min 315Mpa | 440-590Mpa | 22% | 0 | 46J | |
The min impact energy is longitudinal energy |
If you have any need CCS GRADE AH32 and CCS/AH32 steel plate, please feel free to contact us.