ASTM A516 Grade 60, also commonly written as A516GR.60, A516 Gr.60, A516 GR 60 and ASTM A516/A516M Grade 60 [Grade 415], is the inch-pound Grade 60 designation in ASTM A516/A516M. Grade 415 is the SI designation in the same specification, not a converted Grade 60 value. ASME SA516 Grade 60 (SA-516 or SA-516M Grade 60 or Grade 415) is the corresponding ASME family designation, not merely another spelling of the ASTM name. An ASTM-only certificate does not automatically satisfy a specified SA-516 order, and the reverse is also true. The official product page is ASTM A516 Grade 60.
ASTM A516/A516M does not give a single official “working temperature” or a numerical minimum design metal temperature (MDMT) as a Grade 60 property. Design temperature and MDMT are project and construction-code decisions. For ASME Section VIII, Division 1 carbon-steel vessels, Figure UCS-66 is the usual starting point for whether impact testing is required at the MDMT, and the curve assignment for SA-516 Grade 60 depends on heat-treatment condition.
UCS-66 Curve Assignment Commonly Used for SA-516 Grade 60
The following assignment is the reading of Figure UCS-66 notes widely used in ASME VIII-1 practice and restated in Code-software documentation that quotes those notes. Confirm it in the Figure UCS-66 notes of the governing edition. It is a curve classification, not a ready-made MDMT number; the exemption temperature still depends on governing thickness and on any stress-ratio reduction under UCS-66.1.
| Condition of SA-516 Grade 60 plate | Curve commonly assigned in Fig. UCS-66 | What that means in practice |
|---|---|---|
| Not normalized (as-rolled, unless the edition places the plate elsewhere) | Curve C | Figure UCS-66 lists SA-516 Grades 55 and 60, if not normalized, on Curve C. Grade 70, if not normalized, is listed on Curve B and is not the same assignment |
| Normalized, or quenched and tempered | Curve D | Figure UCS-66 lists SA-516, if normalized or quenched and tempered, on Curve D, regardless of grade |
The specification’s scope language — welded pressure vessels in moderate and lower-temperature service where notch toughness matters — is a scope description, not a published temperature window. Allowable stress at a given temperature is taken from Section II, Part D, Table 1A, not from A516; see the discussion on the ASTM A516 Grade 60 official page and the project’s Code edition. In the Table 1A compilations used here, the VIII-1 line for SA-516 Grade 60 is listed up to 1000 °F (538 °C), with graphite and time-dependent-property notes at the higher temperatures.
Test Temperature Is Not the Same as Design Temperature
If notch toughness is required, the order must state the Charpy test temperature, orientation and acceptance criteria, usually by invoking A20/A20M Supplementary Requirement S5 or the construction-code toughness rule that actually applies. When A20/A20M S5 and the Class III standard tables are invoked for Grade 60, commonly quoted acceptance is 13 ft-lbf (18 J) average of three specimens and 10 ft-lbf (14 J) for one specimen, with a thickness-dependent standard temperature (published compilations list −60 °F for t ≤ 1 in. and −50 °F for thicker plate through 5 in., longitudinal). Those values must still be written on the order. A test temperature is not automatically the equipment’s design temperature or MDMT.
Public compilations and SSAB’s Grade 60 delivery description, as disclosed on ASTM A516 Grade 60, indicate normalizing over 1.50 in. [40 mm] unless otherwise ordered, and normally as-rolled delivery at or below that boundary unless ordered otherwise; in the thinner range requiring notch-toughness testing, they describe normalizing unless the purchaser specifies otherwise. Use the rule in the ordered edition. Normalizing is also what typically moves the UCS-66 assignment from Curve C to Curve D.
Frequently Asked Questions (FAQ)
What is the temperature range of ASTM A516 Grade 60?
ASTM A516 does not specify a single service-temperature window for ASTM A516 Grade 60. Design temperature and MDMT are project requirements. In ASME VIII-1 practice, Figure UCS-66 and the governing thickness set whether impact testing is required at the MDMT, and Table 1A sets allowable stress versus temperature.
Which UCS-66 curve is used for ASTM A516 Grade 60?
In the Figure UCS-66 notes commonly applied, ASTM A516 Grade 60 (as SA-516 Grade 60) is Curve C if not normalized, and Curve D if normalized or quenched and tempered. Confirm the notes in the governing ASME VIII-1 edition. The curve does not, by itself, give a numerical MDMT.
Is there a default Charpy temperature for ASTM A516 Grade 60?
No automatic default applies from the grade name. When A20 S5 and the standard-temperature table are invoked, published compilations list −60 °F for ASTM A516 Grade 60 plate 1 in. and under and −50 °F for thicker plate through 5 in. (longitudinal). The order must still state the temperature to be used.
Does “lower-temperature service” fix a minimum temperature for ASTM A516 Grade 60?
No. That phrase is a scope description of ASTM A516 Grade 60, not a numerical minimum design metal temperature.
For plate to ASTM A516/A516M Grade 60 [Grade 415] or ASME SA-516 Grade 60, please contact Gangsteel with the designation, edition, unit system, delivery condition, dimensions, quantity and any supplementary requirements. Learn more about our pressure-vessel and boiler steel plate at Gangsteel.