CCS GRADE AH36 and CCS/AH36 steel plate supplier

 

Gangsteel export CCS GRADE AH36 and CCS/AH36 steel plate. CCS Grade AH36 is shipbuilding steel Grade Stock. What are CCS/AH36 shipbuilding steel equal grade?

 

Keywords: CCS/AH36 Steel plate, CCS Grade AH36, CCS Grade AH36 steel properties, CCS Grade AH36 equivalent material, CCS Grade AH36 round bar, CCS Grade AH36 steel density

 

Henan Gang iron and steel co., Ltd supply steel grade CCS AH36, CCS DH36, CCS EH36, CCS FH36, CCS AH36, CCS DH32, CCS EH32, CCS FH32, CCS GRADE A, CCS GRADE B, CCS GRADE D, CCS GRADE E. CCS AH40, CCS DH40, CCS EH40, CCS FH40.

 

 

In usual if AH36 steel plate thickness above 50mm, mill request the normalized in hot rolled plate Or control rolled, if above 150mm thickness our mill also could use the electroslag remelting technical in ingot to do for our customers.

 

AH36 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:

Thickness: 6mm to 300mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.

 

Henan Gang iron and steel co., Ltd also could supply super thick steel plate thickness from 100mm to 300mm which beyond nine classification society approval.

 

Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly in our mill cost price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

We sincerely hope old and new customers to visit our mill for a long steel business

 

 

CCS GRADE AH36 and CCS/AH36 steel plate Chemical is max composition of product analysis:

Grade C % Si % Mn % P % S % V % AL % Cr %
 AH36 0.180 0.1-0.5 0.90-1.6 0.035 0.035 0.05-0.10 0.015 0.200
Cu % Mo % Nb % Ni % Ti %      
0.350 0.080 0.02-0.05 0.400 0.020      

 

 

CCS GRADE AH36 and CCS/AH36 steel plate mechanical properties

Grade Thickness(mm) Min Yield (Mpa) Tensile(MPa) Elongation(%) Min Impact Energy
AH36 8mm-50mm Min 355Mpa 490-620Mpa 21% 0  34J
51mm-70mm Min 355Mpa 490-620Mpa 21% 0  41J
71mm-100mm Min 355Mpa 490-620Mpa 21% 0  50J
The min impact energy is longitudinal energy

 

If you have any need CCS GRADE AH36 and CCS/AH36 steel plate, please feel free to contact us soon.

 

CCS GRADE AH36 and CCS/AH36 steel plate supplier